Showing posts with label slumping. Show all posts
Showing posts with label slumping. Show all posts

Sunday, August 9, 2009

Arrow In The Forest


Arrow in the Forest
12" square

I finished piece this weekend. You may recall that I did a step by step on the construction of this piece in a May post.

Once I completed coldworking the edges of the plate it was ready for the next step...slumping.

The square sushi plate mold that I used for this piece is one of my favorites. The shape and the way it slopes when the slump is complete seems so elegant to me. I thought you might enjoy seeing the mold, shown in the picture below. The pink on it is the kiln wash that I've applied. This is a necessary step in the slumping process as the wash prevents the glass from sticking to the mold when it slumps.


This is how the fused blank looks as it sets on top of the mold, prior to being put in the kiln for slumping. Once the correct slumping temperature is reached, the glass 'drops', ok it slumps, into the mold and takes on the shape of the mold.



I used some of my favorite Bullseye glasses for this. I've become quite fond of the richness the mineral green opal shade. It lends itself so well as a compliment to the dark green streakie. And I had a lot of fun with the wine colored 'arrow' accented with yellow and clear glass.

Here's wishing all of you a great week of creativity.

Thursday, July 30, 2009

A Grove Of Trees


A Grove of Trees

I cannot believe I started this piece back in May! However, I am happy to report that it is finished. I completed the coldworking on Tuesday evening and the slump firing in the kiln on Wednesday.

I am really drawn to this color scheme. It's abstract, yet I find the subtle colors define that feeling of a grove of trees. Hope you enjoy it.

Happy creating!

Sunday, February 1, 2009

The Weekend Project

I took this photo of what I've been working on this weekend, right before I put it in the kiln. This is my new design for a bowl. I'm trying one of the techniques I learned in the Patty Gray class I took in November of last year.

For this piece, I cut strips of glass and laid them on the 'side' rather than flat. This gives a different view and effect. I alternated two strips of a blue/clear streaky with one strip of clear glass.

Yesterday I was struggling with glass colors and designs. I started on this yesterday afternoon and after some re-working, this is the final design. I'm trying lots of new things with this piece. The most obvious is laying the cut glass strips on their sides. It proved rather challenging to cut them to be the right size as I was laying this in place. I had to re-work things a couple of time.

The other new approach is I have added copper screen inclusions. The photo only shows three copper inclusions well, but there are 4 (I know that digresses from the three point artistic approach). The fourth inclusion is in the lower right section of the circle and is hard to see because it is small and the flash obscured it. They are sandwiched between two layers of clear glass, top and bottom. It will be interesting to see how this copper reacts to the fusing process. It is my understanding that the copper should take on a rusty, red appearance, but after all I have read about copper inclusions, nothing would surprise me color wise...it could turn blue, or even black (I hope it doesn't turn black, but who knows, maybe I'd like that????).

I just hope that this turns out well and all of my time and effort creating the foundation for this bowl won't go to waste. The firing schedule is extra long because of the thickness; it's about 3/8" deep. I have cold working in front of me if this turns out successful, as that will allow me to finish the edges and make sure I have a nice circle for slumping it into the bowl shape. I'm looking forward to seeing how this turns out....that moment when you open the lid of the kiln and go "Great!" or "Back to the drawing board".